The BIOBUILD project represents a significant advancement in the construction and buildings industry by integrating bio-based phase change materials (bioPCM) into wood for applications like parquet and wallboards. To achieve this, the treatments of solid wood and fibers to facilitate bioPCM impregnation is a key focus area in the project, addressing challenges like enhancing wood permeability and reducing the leaching of bioPCM. This article delves into the methodologies, scientific processes and treatments.

BIOBUILD - Exploring Material Pre-treatments - Picture 1
© SLU

Thermal modification of solid wood and fibres

Thermally modified timber is defined as wood that chemical composition and physical properties have been permanently altered through exposure to high temperatures, typically between 160°C and 230°C, under low-oxygen conditions. This controlled pyrolysis ensures thermal degradation of the wood polymers and modifies the material characteristics. The patented thermo-vacuum (TV) process, commercially known as Termovuoto, was used in this project. The process involves placing the timber in a vacuum chamber where a combination of thermal radiation and forced convection heats the material, effectively altering its chemical and cellular structure.

Compared to unmodified wood, thermally modified timber demonstrates improved dimensional stability, reduced hygroscopicity, and increased durability against biodegradation. These changes occur due to chemical transformations within the wood’s cell walls, particularly the degradation of hemicelluloses, crosslinking of lignin, and increased crystallinity of cellulose. The result is a more stable material that is less prone to moisture absorption, a critical feature for applications involving bioPCM impregnation.

© CNR

Microwave (MW) Treatment for Wood Permeability

Microwave (MW) technology provides another approach to enhancing wood porosity and permeability. By applying high-intensity electromagnetic energy, the MWs generate steam pressure within the wood cells. This pressure ruptures weak points, such as pit membranes and ray cells, creating pathways that allow liquids to penetrate deeply into the wood.

BIOBUILD - Exploring Material Pre-treatments - Picture 3
© SLU

MW system with power supply

In BIOBUILD, the MW treatments were conducted at a frequency of 2.45 GHz, with applied power levels ranging from 3 to 8.5 kW.

Both thermal modification and MW treatment were applied to Norway spruce, Scots pine, beech, and poplar boards to optimize their uptake of an organic phase change material (bioPCM). The treatments were followed by a vacuum-pressure impregnation process to ensure the liquid penetration deeply into the wood. The results highlighted significant differences in the effectiveness of these treatments across different wood species and conditions.

Improved Impregnation Efficiency

Thermal modification demonstrated greater overall effectiveness in enhancing wood permeability and bioPCM uptake compared to MW treatment.

For instance, spruce and poplar treated at 200°C exhibited substantial increase of the wood material porosity.

In contrast, MW treatment was most effective when applied at higher power levels, with spruce responding particularly well at 7-8.5 kW applied power.

These findings underscore the importance of tailoring treatment methods to specific wood species and applications.

BIOBUILD - Exploring Material Pre-treatments - Picture 4
© SLU

Arrangement of solid wood samples (lamellas) in the climate chamber during leaching test

Reduced leaching

Reducing leaching of the bioPCM during exploitation is another critical aspect of the BIOBUILD project. Leaching refers to the loss of impregnated material from the wood during use and a decrease of the thermal efficiency of the material. Thermal modification proved effective in mitigating leaching for certain wood species, such as beech, where the treatment at 200°C significantly reduced the bioPCM loss.

However, the leaching rates varied across species and were influenced by factors like wood structure, chemical composition, and the extent of bioPCM uptake.

Applications

Treated solid wood and fibres will be tested in a real application, i.e., middle layer in three-layer parquets and as components in wallboards.

These pilot-scale experiments aim to validate the long-term performance of the materials and assess their scalability for industrial production.

The integration of bioPCM into wood products offers a promising pathway to enhance thermal efficiency in buildings, aligning with global efforts to reduce energy consumption and combat the climate changes.

© SLU

Colour palette in calibrated light of the thermally modified solid wood, chips and fibres

The BIOBUILD project demonstrates how innovation can replace traditional materials, paving the way for energy efficient and sustainability in buildings. BIOBUILD sets a new benchmark for building materials that align not only with the European Green Deal but global environmental goals.